L-3-(4-吡啶基)-丙氨酸钝化钙钛矿太阳电池界面缺陷
|
刘雯雯 1( ), 胡志蕾 1, 王立 1, 曹梦莎 1, 张晶 1, 张婧 1, 张帅 1( ), 袁宁一 1, 丁建宁 2( )
|
Passiviation of L-3-(4-Pyridyl)-alanine on Interfacial Defects of Perovskite Solar Cell
|
LIU Wenwen 1( ), HU Zhilei 1, WANG Li 1, CAO Mengsha 1, ZHANG Jing 1, ZHANG Jing 1, ZHANG Shuai 1( ), YUAN Ningyi 1, DING Jianning 2( )
|
|
图7. (a)PLA修饰钙钛矿薄膜纯电子注入器件的结构示意图, (b)PLA修饰及参照钙钛矿薄膜纯电子注入器件的SCLC测试结果
|
Fig. 7. (a) Schematic diagram of electron-only perovskite film device with PLA, and (b) SCLC measurements of electron-only perovskite film devices with and without PLA
|
|
|
|
|