用固相和水热结合法制备LiMn0.4Fe0.6PO4/C复合材料
|
李荐1,2,3, 姚书恒1, 周宏明1,2,3, 耿文俊1 |
Preparation of LiMn0.4Fe0.6PO4/C Composite by A New Route Combining Solid-state Reaction with Hydrothermal Synthesis
|
LI Jian 1,2,3, YAO Shu-Heng 1, ZHOU Hong-Ming 1,2,3, GENG Wen-Jun 1
|
|
Fig. 1 XRD patterns for a mixture of raw materials sintered at 400 ℃ for 4 h a, at 500 ℃ for 4 h b and at 400 ℃ for 4 h, and then heated at 180 ℃ for 24 h in distilled water c |
|
|
|
|
|