固体氧化物燃料电池的纳米结构阴极的稳定性
洪涛, 王瑶, 夏长荣

Nano-structure Effect on Solid State Fuel Cells Cathode Durability
HONG Tao, WANG Yao, XIA Chang-Rong
图5 LSC-SDC浸渍电极和传统电极在热处理后的600℃极化阻抗 [ 7 ]
Fig. 5 Area specific resistance ASR at 600℃ for the impregnated electrode and the conventional LSC-SDC electrode after heat treatment [ 7 ]