图9 1000℃烧结 2 h 后 SrCo 0.8 Ga 0.2 O 3- #cod#x003b4; 电极与电解质横断面的SEM照片
Fig. 9 Cross-sectional SEM micrograph of SrCo 0.8 Ga 0.2 O 3- #cod#x003b4; electrode and electrolyte sintered at 1000℃ for 2 h