图3 A共轴静电纺装置机理图, B核溶液被辛烷萃取后的未烧结的中空纳米纤维透射电镜照片, C在空气中500℃烧结后所得到锐钛矿TiO 2 中空纳米纤维透射电镜照片, D取向排列的锐钛矿TiO 2 中空纳米纤维扫描电镜照片 [ 8 , 9 ] Fig. 3 A Schematic illustration of the setup for coaxial electrospinning hollow nanofibers, B TEM image of two as-spun hollow fibers after the oily cores extracted with octane, C TEM image of TiO2 anatase hollow fibers that were obtained by calcining the composite nanotubes in air at 500℃, D SEM image of aligned arrays of anatase hollow nanofibers [ 8 , 9 ] |