氧化钇掺杂锆铈酸钡质子导体的制备及性能研究
江虹1,2, 郭瑞松1, 徐江海3, 高沿英1, 邓雅平1

Preparation and Properties of Yttrium Doped Barium Zirconate-cerate Proton Conductors
JIANG Hong1,2, GUO Rui-Song1, XU Jiang-Hai3, GAO Yan-Ying1, DENG Ya-Ping1
图3 试样C3与C3-Z2断面的SEM照片
Fig. 3 SEM images of the fracture section of sample C3 sintered at 1600℃ for 4 h and sample C3-Z2 sintered at 1450℃ for 6 h