钛表面激光熔覆原位制备Ti5Si3涂层结构及摩擦学性能
郭纯1,2, 周健松1, 陈建敏1

Microstructure and Tribological Properties of Ti5Si3CoatingIn-situSynthesized on Titanium Substrate by Laser Cladding
GUO Chun1,2, ZHOU Jian-Song1, CHEN Jian-Min1
图13 对偶GCr15在不同滑动速度下磨损表面形貌和元素面分布图
Fig. 13 SEM micrographs and the corresponding EDS element surface distribution of the worn surface of the counterbody GCr15 steel ball a Sliding speed 0.025 ms; b Sliding speed 0.2 ms normal load of 10 N