新型复合支撑体共烧制备致密La0.7Ca0.3Cr0.97O3-δ连接体薄膜
|
王松林1,2, 凤仪2, 王东生1, 孟广耀3 |
Fabrication of Dense La0.7Ca0.3Cr0.97O3-δ Interconnect Membrane on Novel SOFC Composite Support by Co-firing
|
WANG Song-Lin 1,2, FENG Yi 2, WANG Dong-Sheng 1, MENG Guang-Yao 3
|
|
图1 粉体及烧结样品的XRD图谱 Fig. 1 XRD patterns of the powders and sintered specimen a LCC97 powder; b NiO powder; c NiOLCC97 1:1 sintered at 1400℃ for 4 h |
|
|
|
|
|