Na2O-B2O3-SiO2玻璃焊料连接碳化硅陶瓷接口抗热震性能 |
罗朝华 |
Thermal Shock Behavior of the SiC-SiC Joints Joined with Na2O-B2O3-SiO2 Glass Solder |
图1 不同温度下淬火后中间层界面处微观结构 Fig. 1 Microstructures of the side view of the joint after quenching at different temperatures a 150℃; b 320℃; c 420℃; d 520℃ |