Na2O-B2O3-SiO2玻璃焊料连接碳化硅陶瓷接口抗热震性能
罗朝华12, 江东亮1, 张景贤1, 林庆玲1, 陈忠明1, 黄政仁1

Thermal Shock Behavior of the SiC-SiC Joints Joined with Na2O-B2O3-SiO2 Glass Solder
LUO Zhao-Hua12, JIANG Dong-Liang1, ZHANG Jing-Xian1, LIN Qing-Ling1, CHEN Zhong-Ming1, HUANG Zheng-Ren1
图3 不同温度淬火后试样断面光学照片
Fig. 3 Optical photos of the fracture surface of the specimen after quenching at different temperatures a150℃; b320℃; c420℃; d520℃