Journal of Inorganic Materials

• Research Paper • Previous Articles     Next Articles

Synthesis of Composite AIN Powder Mixed with Sintering Additives by the Lanxide Method

LIN Zhi-Lang1,3; ZHENG Xin-He2; WANG Qun3; ZHOU Mei-Ling3   

  1. 1. Ion Beam Laboratory; Shanghai Institute of Microsystem and Information Technology; Chinese Academy of Sciences; Shanghai 200050; China; 2. Institute of Semiconductors; Beijing 100083, China; 3. School of Materials Science and Engineering; Beijing Polytechnic University; Beijing 100022; China
  • Received:2002-10-18 Revised:2002-12-06 Published:2003-11-20 Online:2003-11-20

Abstract: Composite AlN powder, mixed with the sintering additive Y_2O_3, was synthesized by the direct
nitridation of molten Al-Mg-Y alloys. The character of products was determined by means of electron microscopy, X-ray diffraction,
granularmetric analysis and chemical composition analysis etc. The results show that the nitridation rate of the raw alloys is higher,
and the nitridation products are porous enough to be easily crushed. Composite AlN powder, obtained by the Lanxide method, has excellent
characters such as high purity, especially low oxygen content, and narrow well-distributed grain size and so on.

Key words: AIN powder, Lanxide method, aluminium alloys, sintering additives

CLC Number: