Preparing Process and Sintering Behavior of Nano LaAlO3 Powders

LI Wei; ZHUO Ming-Wen; SHI Jian-Lin; WANG Yi-Lin; KAN Yan-Mei; WANG Ling   

  1. Shanghai Institute of Ceramics; Chinese Academy of Sciences; Shanghai 200050; China
  • Received:2003-04-02 Revised:2003-05-21 Published:2004-05-20 Online:2004-05-20

Abstract: Preparing process and sintering behavior of nano LaAlO3 powders were investigated. The coprecipitation method was applied to synthesize nano LaAlO3 powders. By using La(NO3)3 and Al(NO3)3 as raw materials and keeping pH≈9, the coprecipitation process can be finished at room temperature. Pure LaAlO3 nano powders with a size of about 50nm can be obtained after calcining at 800℃ for 2h. After dry pressing with a pressure of 300MPa, the nano LaAlO3 powders can be sintered at 1500℃ for 4h, and a high density of about 6.2g/cm3 reached.

Key words: LaAlO3, nano, powder, sinter