Formation and Oxidation Behavior of β-Sialon-Melilite Solid Solution Ceramics

ZHANG Jun-Hong; WANG Pei-Ling; JIA Ying-Xin; ZHANG Jiong   

  1. State Key Lab of High Performance Ceramics and Soperfine Microstructhure; Shanghai Institute ofCeramics; Chinese Academy of Sciences Shanghai 200050 China
  • Received:1997-11-13 Revised:1998-01-08 Published:1998-12-20 Online:1998-12-20

Abstract: The formation behavior of the composition of β10-Sialon(Si5.23Al0.77O0.77N7.23) plus 7.26wt% Nd-melilite solid solution (Nd2Si2AlO4N3) prepared by
pressureless sintering was studied. Nd ions in the composition enter α-sialon at low temperature, dissolve in the liquid phase of the material with
temperature increasing. Melilite solid solution can be formed as a grain boundary phase of the ceramics by heat-teatment at 1550℃ for 24h. The oxidation behavior
of the hot-pressed and post-sintered samples was also investigated in the range of 1000~400℃. The melilite solid solution doesn’t caues severe cracking
of the material in oxidation at 1000℃ At high temperature, the oxidized surface of the sample contains preferentially oriented A-Nd2Si2O7 grains and bubbles,
which are formed because of the decrease of the silicate viscosity, incurred by the accumulation of Nd ions to the surface.

Key words: β-sialon, melilite, oxidation behavior