Preparation and Stability of Calcium Cadmium Hydroxyapatite

QIAN Guang-Ren, BAI Hong-Mei, SUN Fu-Cheng, ZHOU Ji-Zhi, SUN Wei-Min, XU Xia   

  1. School of Environment and Chemistry Engineering, Shanghai University, Shanghai 200072, China
  • Received:2007-10-15 Revised:2007-12-20 Published:2008-09-20 Online:2008-09-20

Abstract: Calcium cadmium hydroxyapatites with various Cd doping (Cd/(Cd+Ca))were synthesized and characterized by X-ray diffraction, FT-IR spectroscope and FESEM. TG-DTG-DSC-MS and Toxicity Characteristic Leaching Procedure (TCLP) were used to determine their thermal and chemical stability. The results show that Cd2+ enters into the hydroxyapatites crystal lattice. And
with molar ratios of Cd/(Cd+Ca) increasing, there forms the phases of Ca3.9(Ca4.7Cd0.7)(PO4)6(OH)1.8, Ca{3.8(Ca4.1Cd0.73)(PO4)6(OH)1.8, Ca3.6(Ca4.5Cd0.76)(PO4)6(OH)1.6, Cd5(PO4)3OH, respectively. All the calcium cadmium hydroxyapatites are thermal stable up to 500℃, and their thermal stabilities are enhanced with the increase
of Cd doping, but their chemical stabilities become worse.

Key words: calcium cadmium hydroxyapatite, thermal stability, chemical stability