无机材料学报 ›› 2023, Vol. 38 ›› Issue (11): 1265-1270.DOI: 10.15541/jim20230214

所属专题: 【结构材料】陶瓷基复合材料(202312)

• 研究论文 • 上一篇    下一篇

残余拉应力的温度依赖性及其对裂纹扩展行为的影响

李海燕1,2(), 旷峰华2, 吴昊龙1,2, 刘小根1,2, 包亦望1,2(), 万德田1,2()   

  1. 1.中国国检测试控股集团股份有限公司, 北京 100024
    2.绿色建材国家重点实验室, 中国建筑材料科学研究总院, 北京 100024
  • 收稿日期:2023-05-05 修回日期:2023-06-02 出版日期:2023-06-15 网络出版日期:2023-06-16
  • 通讯作者: 包亦望, 教授. E-mail: ywbao@ctc.ac.cn;
    万德田, 教授. E-mail: dtwan@ctc.ac.cn
  • 作者简介:李海燕(1989-), 女, 博士. E-mail: lihaiyan@ctc.ac.cn
  • 基金资助:
    国家重点研发计划(2021YFB3702300);国家自然科学基金(52032011);国家自然科学基金(52072356);北京市科学技术协会青年人才托举工程

Temperature Dependence of Residual Tensile Stresses and Its Influences on Crack Propagation Behaviour

LI Haiyan1,2(), KUANG Fenghua2, WU Haolong1,2, LIU Xiaogen1,2, BAO Yiwang1,2(), WAN Detian1,2()   

  1. 1. China Building Material Test & Certification Group Co., Ltd., Beijing 100024, China
    2. State Key Laboratory of Green Building Materials, China Building Materials Academy, Beijing 100024, China
  • Received:2023-05-05 Revised:2023-06-02 Published:2023-06-15 Online:2023-06-16
  • Contact: BAO Yiwang, professor. E-mail: ywbao@ctc.ac.cn;
    WAN Detian, professor. E-mail: dtwan@ctc.ac.cn
  • About author:LI Haiyan(1989-), female, PhD. E-mail: lihaiyan@ctc.ac.cn
  • Supported by:
    National Key R&D Program of China(2021YFB3702300);National Natural Science Foundation of China(52032011);National Natural Science Foundation of China(52072356);Young Elite Scientists Sponsorship Program by BAST

摘要:

为研究以高膨胀系数的陶瓷为涂层, 低膨胀系数的陶瓷为基体的预应力陶瓷的高温力学性能, 本工作以氧化锆为涂层, 氧化铝为基体, 制得表层为拉应力的“三明治”结构ZrO2-Al2O3(简称ZcAs)预应力陶瓷。同时选用基体与涂层截面比值相近的Al2O3-ZrO2(简称AcZs)预应力陶瓷、纯ZrO2和纯Al2O3陶瓷为参照样。结合不同温度下的弯曲强度测试结果及维氏压痕结果, 阐明预应力的存在形式及其对裂纹扩展行为的影响, 并研究预应力的温度依赖性。结果表明: ZcAs预应力陶瓷的表层受拉应力, 基体受压应力; 而AcZs预应力陶瓷的表层受压应力, 基体受拉应力。由于拉应力能够促进裂纹扩展, 而压应力能够抑制裂纹扩展, 因此室温下, ZcAs的强度比纯Al2O3陶瓷降低13.2%, 而AcZs的强度比纯ZrO2陶瓷提高25.0%。此外, 无论表层是拉应力还是压应力, 都随着温度升高而降低, 这主要归因于高温导致的预应力松弛。

关键词: ZrO2-Al2O3预应力陶瓷, 拉应力, 弯曲强度, 温度依赖性

Abstract:

To study the mechanical properties at high temperature of pre-stressed ceramics which were prepared by using higher expansion coefficient materials as coating and lower expansion coefficient materials as substrate, zirconia and alumina were chosen as the coating and the substrate, respectively, to fabricate ZrO2-Al2O3 (marked as ZcAs) pre-stressed ceramics with sandwich structure. Meanwhile, Al2O3-ZrO2 pre-stressed ceramics (marked as AcZs, which has the similar section ratio between substrate and coating to ZcAs), ZrO2 ceramics and Al2O3 ceramics were set as the reference samples. Combining the results of bending strength at different temperatures with the results of Vickers indentation, the existence form of residual stress and its influence on crack propagation behavior were clarified as well as the temperature dependence of residual stress. Results show that the residual tensile stress exists in the surface layer of ZcAs, while the compressive stress exists in the substrate. On the contrary, the compressive stress exists in the surface layer of AcZs and tensile stress exists in the substrate. Due to tensile stress promoting while compressive stress inhibiting crack growth, flexural strength of ZcAs is 13.2% lower than that of Al2O3, and AcZs possesses strength 25.0% higher than that of ZrO2 at room temperature. In addition, both tensile stress and compressive stress are decreased with the increase of temperature, which is mainly attributed to the relaxation of pre-stress caused by high temperature.

Key words: ZrO2-Al2O3 pre-stressed ceramics, tensile stress, flexural strength, temperature dependence

中图分类号: